[an error occurred while processing this directive]
AZ31镁合金室温多道次压缩过程微观组织和织构演变的研究
邓丽萍1,崔凯旋2,汪炳叔2(),向红亮1,李强2
Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature
Liping DENG1,Kaixuan CUI2,Bingshu WANG2(),Hongliang XIANG1,Qiang LI2

图6. TD3.0%-RD3.0%-ND3.1%样品孪晶细化晶粒行为EBSD取向成像图和{0001}极图分析

Fig.6. Analyses of the twins refine grains with EBSD orientation mapping (a) and {0001} pole figure (b) (M— matrix, TTD—twin generated from M in 1st compression, TRD1—twin generated from M in 2nd compression, TRD2 and TRD3—twins generated from TTD in 2nd compression, TND—twin generated from TRD3 in 3rd compression)Color online