AZ31镁合金室温多道次压缩过程微观组织和织构演变的研究
邓丽萍1,崔凯旋2,汪炳叔2(),向红亮1,李强2
Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature
Liping DENG1,Kaixuan CUI2,Bingshu WANG2(),Hongliang XIANG1,Qiang LI2

图3. 样品沿TD5.5%-RD5.0%-ND5.2%路径压缩的取向成像图和界面结构图

Fig.3. Orientation image maps (a, c, e) and boundary structure maps (b, d, f) for TD5.5% sample (a, b), TD5.5%-RD5.0% sample (c, d) and TD5.5%-RD5.0%-ND5.2% sample (e, f) (Insets show {0001} pole figures. The red lines indicate {101ˉ2} twin boundaries, and the blue lines indicate boundaries between two {101ˉ2} twin variants within a single grain)