[an error occurred while processing this directive]
C含量对Fe-Mn-Al-C低密度钢组织和性能的影响
陈兴品1(),李文佳1,任平1,曹文全2,刘庆1
Effects of C Content on Microstructure and Properties ofFe-Mn-Al-C Low-Density Steels
Xingpin CHEN1(),Wenjia LI1,Ping REN1,Wenquan CAO2,Qing LIU1

图5. 含C量为0.53%的实验用钢中奥氏体与铁素体两相变形前后的EBSD图

Fig.5. EBSD maps of austenite (a, c) and ferrite (b, d) in the 0.53%C steel before (a, b) and after (c, d) deformation (The numbers 1~5 indicate the aspect ratios of the grains)