核聚变堆用W及其合金辐照损伤行为研究进展
|
|
Research Progress in Irradiation Damage Behavior of Tungsten and Its Alloys for Nuclear Fusion Reactor
|
|
图7. 快中子辐照下W中显微组织演变原理图[ |
Fig.7. Schematic microstructural evolution sequence for fast neutron irradiation of W (Circles represent voids, black loops represent interstitial dislocation loops, red sticks represent elongated Re-rich precipitates)[ |
![]() |