[an error occurred while processing this directive]
TiC含量对铁基复合材料力学性能及耐磨性能的影响
董虎林,包海萍,彭建洪()
Effect of TiC Contents on Mechanical Properties and Wear Resistance of Iron-Based Composites
Hulin DONG,Haiping BAO,Jianhong PENG()

图6. 2.5 kg载荷下纯灰铸铁和原位TiC颗粒增强的铁基复合材料磨损表面形貌的SEM像

Fig.6. SEM images of the worn surfaces of pure grey casting iron (a) and in situ TiC particle reinforced iron-based composite materials 20%TiC/Fe (b), 30%TiC/Fe (c), 40%TiC/Fe (d) and 50%TiC/Fe (e) under load of 2.5 kg (Arrows show the wear directions)