基于中间过渡层的 5A06/0Cr18Ni10Ti 气化冲击焊接工艺研究
|
|
Study on Vaporizing Foil Actuator Welding Process of 5A06/0Cr18Ni10Ti with Interlayer
|
|
图10. 图9b和c中3003/0Cr18Ni10Ti界面不同位置元素线分布 |
Fig.10. Element distributions of the 3003/0Cr18Ni10Ti interface at different areas along line 1 in Fig.9b (a) and line 2 in Fig.9c (b)Color online |
![]() |