基于中间过渡层的 5A06/0Cr18Ni10Ti 气化冲击焊接工艺研究
|
|
Study on Vaporizing Foil Actuator Welding Process of 5A06/0Cr18Ni10Ti with Interlayer
|
|
图9. 能量输入7 kJ时3003/0Cr18Ni10Ti界面形貌的SEM像 |
Fig.9. SEM images of 3003/0Cr18Ni10Ti interface with 7 kJ energy input(a) unwelded area(b) intermetallic compound bonding area showed by rectangle areas(c) element diffusion bonding area |
![]() |