基于中间过渡层的 5A06/0Cr18Ni10Ti 气化冲击焊接工艺研究
|
|
Study on Vaporizing Foil Actuator Welding Process of 5A06/0Cr18Ni10Ti with Interlayer
|
|
图8. 不同能量输入下5A06/3003界面形貌OM像 |
Fig.8. OM images of 5A06/3003 interface with energy inputs of 5 kJ (a), 7 kJ (b) and 9 kJ (c) |
![]() |