[an error occurred while processing this directive]
含水条件下单晶Cu的应力松弛及弹性恢复
史俊勤1,孙琨2,方亮2,许少锋3()
Stress Relaxation and Elastic Recovery of Monocrystalline Cu Under Water Environment
Junqin SHI1,Kun SUN2,Liang FANG2,Shaofeng XU3()

图1. 含水条件下的单晶Cu纳米压入初始模型

Fig.1. The initial model of nanoindentation of monocrystalline copper under water environmentColor online