| Rolling cycle | position | Point | Euler angle (φ1, φ, φ2) | Maximum (SM) | Secondary (SS) | ? / % |
|---|
| First cycle | Surface-{111} | P1 | (358.82, 36.219, 49.918) | 0.4317 | 0.3962 | 8.2233 | | | P2 | (1.6153, 35.251, 47.642) | 0.4251 | 0.3924 | 7.6923 | | | P3 | (3.5297, 35.013, 46.584) | 0.4219 | 0.3954 | 6.2811 | | Surface-{100} | P1 | (97.475, 36.196, 2.1378) | 0.2836 | 0.2677 | 5.6064 | | | P2 | (97.253, 36.315, 3.9174) | 0.2844 | 0.2695 | 5.2391 | | | P3 | (97.851, 36.060, 3.2431) | 0.2871 | 0.2693 | 6.1999 | | Center-{111} | P1 | (203.06, 39.914, 17.290) | 0.4657 | 0.3956 | 15.0526 | | | P2 | (201.92, 40.490, 17.615) | 0.4663 | 0.3926 | 15.8052 | | | P3 | (201.61, 40.022, 18.037) | 0.4675 | 0.3956 | 15.3796 | | Center-{100} | P1 | (277.21, 20.078, 87.222) | 0.3669 | 0.3375 | 8.0130 | | | P2 | (278.54, 20.308, 86.565) | 0.3690 | 0.3344 | 9.3766 | | | P3 | (279.73, 20.075, 85.354) | 0.3702 | 0.3337 | 9.8595 | | Second cycle | Surface-{111} | P1 | (178.23, 33.425, 48.046) | 0.4269 | 0.4063 | 4.8254 | | | P2 | (177.25, 32.668, 48.757) | 0.4305 | 0.4113 | 4.4599 | | | P3 | (176.55, 33.356, 48.129) | 0.4247 | 0.4091 | 3.6731 | | Surface-{100} | P1 | (284.72, 32.614, 74.052) | 0.3013 | 0.2841 | 5.7085 | | | P2 | (287.28, 31.133, 72.346) | 0.3068 | 0.2907 | 5.2477 | | | P3 | (285.63, 31.163, 73.580) | 0.3051 | 0.2887 | 5.3752 | | Center-{111} | P1 | (38.471, 44.421, 2.9263) | 0.4078 | 0.3766 | 7.6508 | | | P2 | (38.870, 44.086, 2.0842) | 0.4073 | 0.3790 | 6.9481 | | | P3 | (39.115, 43.609, 1.7601) | 0.4089 | 0.3773 | 7.7280 | | Center-{100} | P1 | (103.58, 34.267, 86.929) | 0.3067 | 0.2931 | 4.4343 | | | P2 | (102.67, 34.886, 88.888) | 0.3044 | 0.2885 | 5.2233 | | | P3 | (102.64, 35.064, 88.995) | 0.3037 | 0.2869 | 5.5317 |
|