交叉轧制周期对高纯Ta板变形及再结晶梯度的影响
|
祝佳林 1,刘施峰 1( ),曹宇 1,柳亚辉 1,邓超 1,2,刘庆 1,2
|
Effect of Cross Rolling Cycle on the Deformed and Recrystallized Gradient in High-Purity Tantalum Plate
|
Jialin ZHU 1,Shifeng LIU 1( ),Yu CAO 1,Yahui LIU 1,Chao DENG 1,2,Qing LIU 1,2
|
|
图5. 1和2周期样品表面与中心层{111}与{100}晶粒内部的OIM、GROD-Hyper和KAM分布图
|
Fig.5. OIMs (a1~d1), grain reference orientation deviation-hyper (GROD-Hyper) (a2~d2) and kernel average misorientation (KAM) (a3~d3) maps of {111} and {100} grains at the surface and center layer for 1 and 2 cycle samplesColor online(a1~a3) 1 cycle, surface (b1~b3) 1 cycle, center(c1~c3) 2 cycles, surface (d1~d3) 2 cycles, center |
|
|
|
|