交叉轧制周期对高纯Ta板变形及再结晶梯度的影响
|
|
Effect of Cross Rolling Cycle on the Deformed and Recrystallized Gradient in High-Purity Tantalum Plate
|
|
图2. 1和2周期Ta板沿厚度方向的织构分布图 |
Fig.2. Macrotextures along the thickness direction for cross rolling Ta plate with 1 (a1~a3) and 2 (b1~b3) cycles (Fmax—maximum orientation distribution function (ODF) density)Color online(a1, b1) surface layer (a2, b2) quarter layer (a3, b3) center layer |
![]() |