阳极氧化法制备Zr-17Nb合金表面氧化物纳米管阵列及其性能研究
李玲1,姚生莲1,赵晓丽2,3,杨佳佳1,王野熹1,王鲁宁1,4()
Fabrication and Properties of Anodic Oxide Nanotubular Arrays on Zr-17Nb Alloy
Ling LI1,Shenglian YAO1,Xiaoli ZHAO2,3,Jiajia YANG1,Yexi WANG1,Luning WANG1,4()

图6. 阳极氧化120 min制备纳米管的HRTEM分析及元素分布图

Fig.6. HRTEM and EDS analyses of nanotube prepared by anodizing for 120 minColor online(a) TEM image of single nanotube(b1~b4) element distributions of Zr, Nb, O and F, respectively, on a single nanotube(c) HRTEM image of the region I in Fig.6a on a single nanotube, with the fast Fourier transformation (FFT) of the HRTEM image inserted(d) HRTEM image of the region II in Fig.6a on a single nanotube, with the FFT of the HRTEM image inserted