阳极氧化法制备Zr-17Nb合金表面氧化物纳米管阵列及其性能研究
李玲1,姚生莲1,赵晓丽2,3,杨佳佳1,王野熹1,王鲁宁1,4()
Fabrication and Properties of Anodic Oxide Nanotubular Arrays on Zr-17Nb Alloy
Ling LI1,Shenglian YAO1,Xiaoli ZHAO2,3,Jiajia YANG1,Yexi WANG1,Luning WANG1,4()

图5. Zr-17Nb合金及不同阳极氧化时间制备纳米管阵列前后和阳极氧化120 min制备纳米管阵列450 ℃退火处理前后的XRD谱

Fig.5. XRD spectra of Zr-17Nb alloy and nanotubular arrays prepared by different anodization time (a) and GAXRD spectra of nanotubular arrays prepared by anodizing for 120 min before and after annealing at 450 ℃ (b)