阳极氧化法制备Zr-17Nb合金表面氧化物纳米管阵列及其性能研究
李玲1,姚生莲1,赵晓丽2,3,杨佳佳1,王野熹1,王鲁宁1,4()
Fabrication and Properties of Anodic Oxide Nanotubular Arrays on Zr-17Nb Alloy
Ling LI1,Shenglian YAO1,Xiaoli ZHAO2,3,Jiajia YANG1,Yexi WANG1,Luning WANG1,4()

图2. Zr-17Nb合金表面不同阳极氧化时间制备的纳米管结构表面和截面形貌的SEM像

Fig.2. Top view (a1~d1) and cross-sectional (a2~d2) SEM images of nanotubular arrays on Zr-17Nb alloy prepared with anodic oxidation time of 10 min (a1, a2), 30 min (b1, b2), 60 min (c1, c2) and 120 min (d1, d2) (Insets in Figs.2a2~d2 show the enlarged views of square areas)