双相钛合金高温变形协调性的CPFEM研究
|
|
Crystal Plasticity Finite Element Method Investigation of the High Temperature Deformation Consistency in Dual-Phase Titanium Alloy
|
|
图3. 局部晶粒结构及750 ℃高温变形云图 |
Fig.3. Contour maps of a group of three grains after high temperature tensile deformation at 750 ℃ |
![]() |