双相钛合金高温变形协调性的CPFEM研究
|
|
Crystal Plasticity Finite Element Method Investigation of the High Temperature Deformation Consistency in Dual-Phase Titanium Alloy
|
|
图1. 双相钛合金多晶几何构型图 |
Fig.1. Grains and phase distribution in dual-phase polycrystalline titanium alloy |
![]() |