[an error occurred while processing this directive]
金属轧制复合过程微观变形行为的分子动力学建模及研究
张清东,李硕,张勃洋(),谢璐,李瑞
Molecular Dynamics Modeling and Studying of Micro-Deformation Behavior in Metal Roll-Bonding Process
Qingdong ZHANG,Shuo LI,Boyang ZHANG(),Lu XIE,Rui LI

图6. 图5中A~B阶段,变形过程中界面处位错向FeCrNi基体发射过程

Fig.6. Atomic configurations (a1, b1, a2, b2) and dislocation distributions (c1, c2) at point A (a1~c1) and point B (a2~c2) in Fig.5 showing the process of dislocation at the interface emitted to the FeCrNi matrix (Red color represents the hcp atoms and two adjacent hcp atoms mean an intrinsic stacking fault)