金属轧制复合过程微观变形行为的分子动力学建模及研究
张清东,李硕,张勃洋(),谢璐,李瑞
Molecular Dynamics Modeling and Studying of Micro-Deformation Behavior in Metal Roll-Bonding Process
Qingdong ZHANG,Shuo LI,Boyang ZHANG(),Lu XIE,Rui LI

图5. 600 K下FeCrNi/Fe沿z方向单轴压缩作用下的应力-应变曲线以及材料变形截图

Fig.5. Stress-strain curve and the sequence of snapshots capturing the atomic deformation process for FeCrNi/Fe under z-direction uniaxial compression at 600 K (The red, blue and yellow colors represent the Fe, Cr and Ni atoms, respectively, in FeCrNi matrix. The white color represents the Fe atoms in Fe matrix)