金属轧制复合过程微观变形行为的分子动力学建模及研究
张清东,李硕,张勃洋(),谢璐,李瑞
Molecular Dynamics Modeling and Studying of Micro-Deformation Behavior in Metal Roll-Bonding Process
Qingdong ZHANG,Shuo LI,Boyang ZHANG(),Lu XIE,Rui LI

图4. 双金属FeCrNi/Fe、单金属FeCrNi和Fe沿z方向压缩的应力-应变曲线

Fig.4. Stress-strain curves for FeCrNi/Fe、FeCrNi and Fe under z-direction compression