B4C/6061Al复合材料热压缩断裂行为的多尺度研究
周丽1,张鹏飞1,王全兆2(),肖伯律2,马宗义2,于涛1
Multi-Scale Study on the Fracture Behavior of Hot Compression B4C/6061Al Composite
Li ZHOU1,Pengfei ZHANG1,Quanzhao WANG2(),Bolü XIAO2,Zongyi MA2,Tao YU1

图2. 热压缩有限元模型

Fig.2. Finite element model for hot compression