B4C/6061Al复合材料热压缩断裂行为的多尺度研究
周丽1,张鹏飞1,王全兆2(),肖伯律2,马宗义2,于涛1
Multi-Scale Study on the Fracture Behavior of Hot Compression B4C/6061Al Composite
Li ZHOU1,Pengfei ZHANG1,Quanzhao WANG2(),Bolü XIAO2,Zongyi MA2,Tao YU1

图10. 随压缩时间的延长,细观模型中裂纹的形成过程

Fig.10. Crack formation in mesoscopic model at time of 0.06 s (a), 0.062 s (b), 0.065 s (c) and 0.068 s (d)