GH984G合金在700 ℃水蒸气中的氧化行为
王常帅1(),郭莉莉1,唐丽英2,周荣灿2,郭建亭1,周兰章1
Oxidation Behavior of GH984G Alloy in Steam at 700 ℃
Changshuai WANG1(),Lili GUO1,Liying TANG2,Rongcan ZHOU2,Jianting GUO1,Lanzhang ZHOU1

图6. GH984G合金在700 ℃蒸汽条件下氧化2000 h后的截面形貌和元素线分布

Fig.6. Cross-section image and line scans of GH984G alloy after oxidiation in steam at 700 ℃ for 2000 h