GH984G合金在700 ℃水蒸气中的氧化行为
王常帅1(),郭莉莉1,唐丽英2,周荣灿2,郭建亭1,周兰章1
Oxidation Behavior of GH984G Alloy in Steam at 700 ℃
Changshuai WANG1(),Lili GUO1,Liying TANG2,Rongcan ZHOU2,Jianting GUO1,Lanzhang ZHOU1

图1. GH984G合金在700 ℃蒸汽条件下的氧化动力学曲线

Fig.1. Oxidation kinetics curves of GH984G alloy in steam at 700 ℃ (Δw—mass gain, t—oxidation time)(a, b) Δw versus t (c) relationship between Δw and t1/2