TC11/TC17
钛合金线性摩擦焊接头界面研究
杜随更(
),高漫,徐婉婷,王喜锋
Study on Interface of Linear Friction Welded Joint Between TC11 and TC17 Titanium Alloy
Suigeng DU(
),Man GAO,Wanting XU,Xifeng WANG
图1.
TC11和TC17显微组织
Fig.1.
Microstructures of TC11 (a) and TC17 (b) alloys