电磁旋流水口连铸技术对小方坯凝固组织形貌和宏观偏析的影响
|
|
Influence of Electromagnetic Swirling Flow in Nozzle on Solidification Structure and Macrosegregation of Continuous Casting Square Billet
|
|
图6. 不同实验条件下硫印检验结果 |
Fig.6. Sulfur segregation spots distributings after sulfur print under different conditions(a) EMSFN, 200A (b) EMSFN, 400 A (c) EMSFN, 600 A (d) M-EMS |
![]() |