电磁旋流水口连铸技术对小方坯凝固组织形貌和宏观偏析的影响
|
|
Influence of Electromagnetic Swirling Flow in Nozzle on Solidification Structure and Macrosegregation of Continuous Casting Square Billet
|
|
图1. 工业实验中EMSFN设备、M-EMS、SEN与结晶器的结构与尺寸示意图 |
Fig.1. Dimension and structure schematic of EMSFN device, M-EMS, SEN and mold applied in industrial test (EMSFN—electromagnetic swirling flow in nozzle, M-EMS—mold electromagnetic stirrer, SEN—submerged entry nozzle) |
![]() |