[an error occurred while processing this directive]
静水压力对超纯Fe腐蚀行为的影响
马荣耀1,2,王长罡1,穆鑫1,魏欣1,赵林1,董俊华1(),柯伟1
Influence of Hydrostatic Pressure on Corrosion Behavior of Ultrapure Fe
Rongyao MA1,2,Changgang WANG1,Xin MU1,Xin WEI1,Lin ZHAO1,Junhua DONG1(),Wei KE1

图8. 0.1和10 MPa静水压力下超纯Fe在3.5%NaCl中0~6.2×104 s内腐蚀事件发生的频率(fn)和腐蚀事件的平均电量(q)随时间的变化图

Fig.8. Plot of the frequency of events (fn) (a) and the average charge in each event (q) (b) versus time for ultrapure Fe exposed to 3.5%NaCl aqueous solution for 0~6.2×104 s at hydrostatic pressures of 0.1 and 10 MPa