[an error occurred while processing this directive]
静水压力对超纯Fe腐蚀行为的影响
马荣耀1,2,王长罡1,穆鑫1,魏欣1,赵林1,董俊华1(),柯伟1
Influence of Hydrostatic Pressure on Corrosion Behavior of Ultrapure Fe
Rongyao MA1,2,Changgang WANG1,Xin MU1,Xin WEI1,Lin ZHAO1,Junhua DONG1(),Wei KE1

图16. 0.1和10 MPa静水压力下,超纯Fe在3.5%NaCl中EPN和ECN的Hilbert边际谱随时间变化图

Fig.16. Time-dependent variation of Hilbert marginal spectra of the EPN (a, b) and ECN (c, d) signal of ultrapure Fe exposed to 3.5%NaCl aqueous solution at hydrostatic pressures of 0.1 MPa (a, c) and 10 MPa (b, d) for a duration of 204.8 s