[an error occurred while processing this directive]
静水压力对超纯Fe腐蚀行为的影响
马荣耀1,2,王长罡1,穆鑫1,魏欣1,赵林1,董俊华1(),柯伟1
Influence of Hydrostatic Pressure on Corrosion Behavior of Ultrapure Fe
Rongyao MA1,2,Changgang WANG1,Xin MU1,Xin WEI1,Lin ZHAO1,Junhua DONG1(),Wei KE1

图14. 0.1和10 MPa静水压力下,0~2.5×104和2.5×104~6.2×104 s内超纯Fe的点蚀生长概率(Pc) -q图

Fig.14. Plots for pitting corrosion growth probabilities (Pc) vs q of ultrapure Fe exposed to 3.5%NaCl solution at hydrostatic pressures of 0.1 and 10 MPa