静水压力对超纯Fe腐蚀行为的影响
马荣耀1,2,王长罡1,穆鑫1,魏欣1,赵林1,董俊华1(),柯伟1
Influence of Hydrostatic Pressure on Corrosion Behavior of Ultrapure Fe
Rongyao MA1,2,Changgang WANG1,Xin MU1,Xin WEI1,Lin ZHAO1,Junhua DONG1(),Wei KE1

图1. 模拟深海腐蚀电化学测试系统示意图

Fig.1. Schematic of simulated deep sea corrosion electrochemical test system (1—high purity nitrogen bottle, 2—autoclave, 3—electrode, 4—thermocouple, 5—pressure transmitter, 6—circulating water jacket, 7—low temperature constant temperature circulating water tank, 8—console, 9—electrochemical workstation)