地质处置低氧过渡期X65低碳钢腐蚀行为研究
|
|
Corrosion Behaivour of X65 Low Carbon Steel During Redox State Transition Process of High LevelNuclear Waste Disposal
|
|
图8. X65低碳钢在80 ℃低氧饱和膨润土中腐蚀不同时间后的表面形貌 |
Fig.8. Surface morphologies of X65 low carbon steel immersed in anoxic saturated bentonite at 80 ℃ for 10 d (a), 50 d (b), 100 d (c) and 150 d (d) |
![]() |