Corrosion Behaivour of X65 Low Carbon Steel During Redox State Transition Process of High LevelNuclear Waste Disposal
|
|
图7. X65低碳钢在80 ℃低氧饱和膨润土中EIS等效电路与物理模型 |
Fig.7. Equivalent circuit and physical model of EIS recorded on X65 low carbon steel in anoxic saturated bentonite at 80 ℃ for 1~40 d (a) and 60~150 d (b) (Rs—corrosion media resistance, Rct—charge transfer resistance, RL—localized corrosion resistance, Rf—film resistance, L—inductance, Qdl—constant phase angle element of electric double layer, Qf—constant phase angle element of electric double layer, W—Warburg resistance) |
![]() |