Mo元素及热处理对Ni2CrFeMox高熵合金在NaCl溶液中耐蚀性能的影响
|
|
Effect of Mo Element and Heat Treatment on Corrosion Resistance of Ni2CrFeMox High-Entropy Alloyin NaCl Solution
|
|
图5. 铸态和热处理态Ni2FeCrMo0.2合金(未被极化腐蚀)的EDS面扫描图 |
Fig.5. EDS maps of as-cast (a) and heat treated (b) Ni2FeCrMo0.2 alloy (unpolarized) |
![]() |