Mo元素及热处理对Ni2CrFeMox高熵合金在NaCl溶液中耐蚀性能的影响
|
|
Effect of Mo Element and Heat Treatment on Corrosion Resistance of Ni2CrFeMox High-Entropy Alloyin NaCl Solution
|
|
图1. 铸态Ni2CrFeMo |
Fig.1. Cyclic polarization curves of the as-cast Ni2Cr-FeMox alloys and 316L stainless steel in 3.5%NaCl solution (Eprot—protection potential, Eb—breakdown potential) |
![]() |