Mo元素及热处理对Ni2CrFeMox高熵合金在NaCl溶液中耐蚀性能的影响 |
|||||||||||||||
| 魏琳,王志军,吴庆峰,尚旭亮,李俊杰,王锦程 | |||||||||||||||
|
Effect of Mo Element and Heat Treatment on Corrosion Resistance of Ni2CrFeMox High-Entropy Alloyin NaCl Solution |
|||||||||||||||
| Lin WEI,Zhijun WANG,Qingfeng WU,Xuliang SHANG,Junjie LI,Jincheng WANG | |||||||||||||||
| 表3 铸态和热处理态Ni2CrFeMo0.2合金中各元素经XPS分析后不同氧化态之间的原子比 | |||||||||||||||
| Table 3 Atomic ratio between different oxidation states of each element in as-cast and heat-treated Ni2CrFeMo0.2 alloy after XPS analysis | |||||||||||||||
|
|||||||||||||||