Mo元素及热处理对Ni2CrFeMox高熵合金在NaCl溶液中耐蚀性能的影响
|
|
Effect of Mo Element and Heat Treatment on Corrosion Resistance of Ni2CrFeMox High-Entropy Alloyin NaCl Solution
|
|
图7. 铸态和热处理态Ni2FeCrMo0.2合金在3.5%NaCl溶液中的EIS |
Fig.7. Nyquist plots (a) and Bode plots (b) of as-cast and heat-treated Ni2FeCrMo0.2 alloys in 3.5%NaCl solution |
![]() |