Mo元素及热处理对Ni2CrFeMox高熵合金在NaCl溶液中耐蚀性能的影响
|
|
Effect of Mo Element and Heat Treatment on Corrosion Resistance of Ni2CrFeMox High-Entropy Alloyin NaCl Solution
|
|
图6. 铸态 Ni2FeCrMox合金在3.5%NaCl溶液中的EIS |
Fig.6. Nyquist plots (a) and Bode plots (b) of as-cast Ni2FeCrMox alloys in 3.5%NaCl solution |
![]() |