Al-Bi合金凝固过程及微合金化元素Sn的影响
|
黎旺 1,2,孙倩 1,2,江鸿翔 1,赵九洲 1,2(  )
|
|
Solidification of Al-Bi Alloy and Influence of Microalloying Element Sn
|
Wang LI 1,2,Qian SUN 1,2,Hongxiang JIANG 1,Jiuzhou ZHAO 1,2(  )
|
|
|
图10. Al-9.0%Bi和Al-9.0%Bi-0.10%Sn合金富Bi相二维平均直径()、数量密度()和随凝固时间的变化
|
Fig.10. 2D average diameters (), number density () and of the Bi-rich droplets as a function of time during a cooling of the Al-9.0%Bi alloy (dash line) and Al-9.0%Bi-0.10%Sn alloy (solid line) (The subscripts 1 and 2 represent the primary droplets and the secondary droplets, respectively) |
|
 |
|
|