Al-Bi合金凝固过程及微合金化元素Sn的影响
|
|
Solidification of Al-Bi Alloy and Influence of Microalloying Element Sn
|
|
图1. Al-9.0%Bi合金熔体冷却曲线 |
Fig.1. Temperature curve of Al-9.0%Bi alloy during cooling (t—cooling time, tα-Al—growth time of α-Al) |
![]() |