Al-Bi合金凝固过程及微合金化元素Sn的影响
黎旺1,2,孙倩1,2,江鸿翔1,赵九洲1,2()
Solidification of Al-Bi Alloy and Influence of Microalloying Element Sn
Wang LI1,2,Qian SUN1,2,Hongxiang JIANG1,Jiuzhou ZHAO1,2()

图3. Al-xBi合金中富Bi相粒子的二维尺寸分布

Fig.3. 2D size distributions of the Bi-rich particles in the Al-xBi alloys with x=5.0% (a), x=7.0% (b), x=9.0% (c) and x=12.0% (d)