Fe-BTC表面氨基化及对染料和重金属离子的吸附性能研究
曹梦薇,蔡桃,张霞()
Study on Amination Modification of Fe-BTC and Their Adsorption for Dyes and Heavy Metal Ions
Mengwei CAO,Tao CAI,Xia ZHANG()

图9. DETA-Fe-BTC去除CR和Pb(II)的循环性能测试

Fig.9. Reusability of DETA-Fe-BTC in the cyclic removal of CR and Pb(II)