Fe-BTC表面氨基化及对染料和重金属离子的吸附性能研究
曹梦薇,蔡桃,张霞()
Study on Amination Modification of Fe-BTC and Their Adsorption for Dyes and Heavy Metal Ions
Mengwei CAO,Tao CAI,Xia ZHANG()

图8. DETA-Fe-BTC对于不同金属离子和染料的吸附量对比

Fig.8. Comparison of adsorption capacity of three metal ions and three dyes using DETA-Fe-BTC as adsorbents