Fe-BTC表面氨基化及对染料和重金属离子的吸附性能研究
曹梦薇,蔡桃,张霞()
Study on Amination Modification of Fe-BTC and Their Adsorption for Dyes and Heavy Metal Ions
Mengwei CAO,Tao CAI,Xia ZHANG()

图6. Fe-BTC 和DETA-Fe-BTC对于CR和Pb(II)的吸附等温线(25 ℃)

Fig.6. Adsorption isotherm of CR (a) and Pb (b) on Fe-BTC and DETA-Fe-BTC at 25 ℃