Fe-BTC表面氨基化及对染料和重金属离子的吸附性能研究
曹梦薇,蔡桃,张霞()
Study on Amination Modification of Fe-BTC and Their Adsorption for Dyes and Heavy Metal Ions
Mengwei CAO,Tao CAI,Xia ZHANG()

图2. Fe-BTC和DETA-Fe-BTC表面Zeta电位随pH值变化曲线以及N2吸附-脱附曲线

Fig.2. The dependence of Zeta potentials upon different pH values (a) and N2 adsorption-desorption isotherms (b) for original Fe-BTC and DETA-Fe-BTC (P—partial pressure of adsorbate, P0—saturated vapor pressure of adsorbent)