基于同步辐射X射线成像的选区激光熔化Ti-6Al-4V合金缺陷致疲劳行为
吴正凯1,吴圣川1(),张杰2,宋哲1,胡雅楠1,康国政1,张海鸥3
Defect Induced Fatigue Behaviors of Selective Laser Melted Ti-6Al-4V via Synchrotron Radiation X-Ray Tomography
Zhengkai WU1,Shengchuan WU1(),Jie ZHANG2,Zhe SONG1,Yanan HU1,Guozheng KANG1,Haiou ZHANG3

图10. 选区激光熔化Ti-6Al-4V合金不同类型缺陷断口形貌特征

Fig.10. Fracture morphologies of different defects in selective laser melted Ti-6Al-4V