基于同步辐射X射线成像的选区激光熔化Ti-6Al-4V合金缺陷致疲劳行为
吴正凯1,吴圣川1(),张杰2,宋哲1,胡雅楠1,康国政1,张海鸥3
Defect Induced Fatigue Behaviors of Selective Laser Melted Ti-6Al-4V via Synchrotron Radiation X-Ray Tomography
Zhengkai WU1,Shengchuan WU1(),Jie ZHANG2,Zhe SONG1,Yanan HU1,Guozheng KANG1,Haiou ZHANG3

图5. 缺陷等效直径的频率直方图及累积频率曲线

Fig.5. Distribution of effective diameter of defects and its cumulative frequency curve