X80管线钢焊接接头的模拟重构及电偶腐蚀行为表征
|
|
Reconstruction and Characterization of Galvanic Corrosion Behavior of X80 Pipeline Steel Welded Joints
|
|
图7. X80钢焊接接头各部分的极化曲线 |
Fig.7. Potentiodynamic polarization curves of X80 steel welded joint |
![]() |