X80管线钢焊接接头的模拟重构及电偶腐蚀行为表征
|
|
Reconstruction and Characterization of Galvanic Corrosion Behavior of X80 Pipeline Steel Welded Joints
|
|
图8. X80钢焊接接头各部分在不同浸泡时间下的极化曲线 |
Fig.8. Potentiodynamic polarization curves of X80 steel (a), ICHAZ (b), FGHAZ (c), CGHAZ (d) and WM (e) |
![]() |