X80管线钢焊接接头的模拟重构及电偶腐蚀行为表征
|
|
Reconstruction and Characterization of Galvanic Corrosion Behavior of X80 Pipeline Steel Welded Joints
|
|
图4. X80钢焊接接头各部分在CO2饱和的NACE溶液中的EIS |
Fig.4. Nyquist diagram (a) and Bode plots (b) of X80 steel welded joint in NACE solution saturated with CO2 (NACE—national association of corrosion engineers) |
![]() |